Inspection
Visually inspect for pitting or erosion in the crevice seal
groove.
Replace the liner if pitting or erosion is greater than
one-half the width of the crevice seal groove.
Visually inspect the outside diameter for excessive cor-
rosion or pitting. Pits must not be more than 1.60 mm
[0.063-inch] deep.
Replace the liner if the pits are too deep or if the corrosion
can not be removed with a fine emery cloth.
Liners which have light pitting or erosion can be used
again, but they must be installed with the pitting or ero-
sion positioned in line with the crankshaft.
Visually inspect for cracks on the inside and the outside
of the liner.
Replace the liner if cracks are found.
Cylinder Liners - Cleaning and Inspection (01-06) Cylinder Block